Polymer Property : 100% Modulus = 1.93 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
100% Modulus 0.0133 GPa
1.93 ksi
ASTM D412
Precision Polymer Engineering Perlast® G70T Perfluoroelastomer
A black perfluoroelastomer compound with excellent steam resistance and mechanical properties. It has extremely low outgassing properties.Applications: For use in applications which require long-ter..
100% Modulus 0.0133 GPa
1.93 ksi
ASTM D412
C.O.I.M. LARIPUR® LPR2202-95A Seal Grade TPU
Description: The products of the LARIPUR® line are thermoplastic polyurethanes. These products combine the technology of thermoplastic products with the features of polyurethanes:Excellent abrasion..