Mechanical Properties Metric English Comments
100% Modulus 0.0134 GPa
1.95 ksi
ASTM D-638
Axiall 12881 Wire & Cable Flexible PVC
Flame retardant, specialty grade, 75°C rated jacket compound. Designed to present a unique clear, sparkling appearance to the finished cable.Information provided by Georgia GulfGeorgia Gulf became..