Mechanical Properties | Metric | English | Comments |
---|---|---|---|
100% Modulus | 0.0151 GPa | 2.19 ksi | ASTM D412 |
Precision Polymer Engineering Perlast® G81T Perfluoroelastomer A special black perfluoroelastomer compound with PTFE blended for improved mechanical performance. Excellent steam resistance and mechanical properties. Extremely low outgassing properties. Applica.. |
|||
100% Modulus | 0.0151 GPa | 2.19 ksi | JIS-A-5756 |
Denka VINYKON W4203 PVC, W grade for equipment cords, for heat resistance A PVC resin compound offering excellent physical properties and workability. A broad product lineup is available, including hard and soft grades, as well as those for extrusion and injection molding.. |