Mechanical Properties Metric English Comments
100% Modulus 0.0156 GPa
2.26 ksi
Die C; Flow direction; ASTM D412
Teknor Apex Sarlink® 4449D Thermoplastic Elastomer
A NSF certified, highly engineered Thermoplastic Elastomer for use in demanding applications. Sarlink® 4449D is a high hardness grade possessing exceptional tensile strength, superior compression..
100% Modulus 0.0156 GPa
2.26 ksi
ASTM D638
Colorite Polymers 9614 General Purpose Vinyl Compound
Description: Colorite produces many vinyl compounds. They have the compounds that perfectly suit whatever the application. Requirements such as ultraviolet ray resistance, fungus resistance, flame r..
100% Modulus 0.0156 GPa
2.26 ksi
Die C; Flow direction; ASTM D412
Teknor Apex Sarlink® 4149D Thermoplastic Elastomer
A highly engineered Thermoplastic Elastomer for use in demanding applications. Sarlink® 4149D is a high hardness grade possessing exceptional tensile strength, superior compression set, chemical re..