Mechanical Properties | Metric | English | Comments |
---|---|---|---|
100% Modulus | 0.0163 GPa | 2.36 ksi | ASTM D412 |
Precision Polymer Engineering Perlast® G80T Perfluoroelastomer A black perfluoroelastomer compound with excellent steam resistance and mechanical properties. It has extremely low outgassing properties.Applications: For use in applications which require long-ter.. |