Polymer Property : 100% Modulus = 2.90 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
100% Modulus 0.0200 GPa
2.90 ksi
ASTM D412
S&E Specialty Polymers GA-1046CTLF PVC
Application: Lead free 105° C tri-rated semi-rigid insulation compound suitable for UL style 1061, CSA-SRPVC, MIL-I-16878.Information provided by S&E Specialty Polymers
100% Modulus 0.0200 GPa
2.90 ksi
DIN 53.504
Lubrizol Advanced Materials Pearlthane® Clear 15N60D Thermoplastic Polyurethane  (discontinued **)
Polyester-based TPU, supplied in form of translucent, colorless or slightly yellowish pellets, combining very high hardness with excellent mechanical properties and excellent hyrdrolysis resistance...
100% Modulus 0.0200 GPa
2.90 ksi
ASTM D412
Lubrizol Pellethane® 2363-65D Thermoplastic Polyurethane Elastomer
Feature: USP Class VIAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Pellethane product line from Dow in 2009.
100% Modulus 0.0200 GPa
2.90 ksi
ISO 37
Lubrizol ESTANE® GP60DE Ester Based Thermoplastic Polyurethane
Estane® GP 60DE is an aromatic polyester-based thermoplastic polyurethane (TPU).Appearance: Translucent spherical pelletsUses: Injection molding partsAvailable in EuropeInformation provided by Lubr..
100% Modulus 0.0200 GPa
2.90 ksi
Elastomer Engineering E60D Polyurethane
A polyester-based urethane with particularly high load-bearing characteristics. Information provided by Elastomer Engineering Inc (EEI)
100% Modulus 0.0200 GPa
2.90 ksi
ASTM D412
Lubrizol Estane® 2102-65D Thermoplastic Polyurethane Elastomer
Formerly PellethaneAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Pellethane product line from Dow in 2009.
100% Modulus 0.0200 GPa
2.90 ksi
AdvanSource Biomaterials ChronoFlex® AL 55D Biodurable Medical Grade Polyurethane
ChronoFlex® AL is a family of premium polycarbonate aliphatic biodurable thermoplastic polyurethane elastomers developed by  AdvanSource Biomaterials Corporation. ChronoFlex® AL medical-grade el..
100% Modulus 0.0200 GPa
2.90 ksi
ASTM D-638
Axiall 15642 Wire & Cable Flexible PVC
Non-lead stabilized semi-rigid insulation compound recommended for Style #1061 applications. Maximum service temperature of 105°C.Information provided by Georgia GulfGeorgia Gulf became Axiall Cor..
100% Modulus 0.0200 GPa
2.90 ksi
ASTM D-638
Axiall 15644 Wire & Cable Flexible PVC
Semi-rigid insulation compound recommended for Style #1061 applications. Maximum service temperature of 105°C.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.