Mechanical Properties Metric English Comments
100% Modulus 0.0203 GPa
2.95 ksi
ASTM D-638
Axiall 15640 Wire & Cable Flexible PVC
Semi-rigid UL style #1061.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
100% Modulus 0.0203 GPa
2.95 ksi
ASTM D-638
Axiall 22560 Coax & Telecom Flexible PVC
Semi-rigid thinwall insulation. 6+ mils.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.