Mechanical Properties Metric English Comments
Tensile Impact Strength 273 kJ/m²
130 ft-lb/in²
ASTM D1822
ExxonMobil HDPE HD 9830.02 High Density Polyethylene Resin
Product Description: HD 9830.02 is a blow molding grade high density polyethylene copolymer with a bimodal molecular weight distribution. It provides a very good balance of stress crack resistance, ..
Tensile Impact Strength 273 kJ/m²
130 ft-lb/in²
Molded and tested in accordance with ASTM D4976; ASTM D1822, Type S
Dow 722 Linear Low Density Polyethylene (LDPE)
DOW Polyethylene 722 is a broad molecular weight distribution homopolymer designed to offer good impact strength and rack resistance, with excellent flexibility. Typical applications include caps/c..