Polymer Property : Tensile Impact Strength = 138.2 kJ/m² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Impact Strength 138.2 kJ/m²
65.76 ft-lb/in²
At 23°C; ASTM D1822S
DuPont Nucrel® 2906 Ethylene-Methacrylic Acid Copolymer Resin  (discontinued **)
Nucrel® 2906 is a tough, lightweight, easily processed ethylene copolymer resin. This resin is inherently flexible without the need for plasticizers. The resin can be pigmented, UV-stabilized for..