Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Impact Strength | 130 - 353 kJ/m² | 61.9 - 168 ft-lb/in² | Average value: 221 kJ/m² Grade Count:4 |
Overview of materials for Medium Density Polyethylene (MDPE), Molded This property data is a summary of similar materials in the MatWeb database for the category "Medium Density Polyethylene (MDPE), Molded". Each property range of values reported is minimum and maxim.. |