Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Impact Strength | 360 kJ/m² | 171 ft-lb/in² | 23°C; ASTM D-1822 |
ExxonMobil Optema® TC-020 Ethylene Methyl Acrylate for Injection Molding
(discontinued **) Data provided by the manufacturer, Exxon Chemical.6.5% Methyl Acrylate. An Ethylene Methyl Acrylate copolymer which can be injection molded to produce pliable parts. It can also be used for making.. |