Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Impact Strength | 40.0 - 80.0 kJ/m² | 19.0 - 38.1 ft-lb/in² | Average value: 56.7 kJ/m² Grade Count:3 |
Overview of materials for Liquid Crystal Polymer (LCP), Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), Mineral Filled". Each property range of values reported is minimum and max.. |
|||
Tensile Impact Strength | 39.9 kJ/m² | 19.0 ft-lb/in² | |
ITW Devcon Flex Welderâ„¢ Methacrylate Adhesive FC, Off-White, Black Information provided by ITW Devcon |