Mechanical Properties Metric English Comments
Tensile Impact Strength 472 kJ/m²
225 ft-lb/in²
Type S; ASTM D1822
SABIC Innovative Plastics Lexan® HP2R PC
Med/High flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains a..
Tensile Impact Strength 472 kJ/m²
225 ft-lb/in²
Type S; ASTM D1822
SABIC Innovative Plastics Lexan® HPS2 PC
Med/high flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam, e-beam and gamma sterilizable..
Tensile Impact Strength 472 kJ/m²
225 ft-lb/in²
Type S; ASTM D1822
SABIC Innovative Plastics Lexan® HPS2 PC (Asia Pacific)
Med/high flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam, e-beam and gamma sterilizable..
Tensile Impact Strength 472 kJ/m²
225 ft-lb/in²
Type S; ASTM D1822
SABIC Innovative Plastics Lexan® HPS2R PC
Med/high flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam, e-beam and gamma sterilizable..
Tensile Impact Strength 472 kJ/m²
225 ft-lb/in²
Type S; ASTM D1822
SABIC Innovative Plastics Lexan® LS1 PC
UL rated HB as of 10/97. 200 series recommended when V-2 rating required. Automotive lens applications. Low viscosity. UV-stabilized. Transparent colors only.
Tensile Impact Strength 472 kJ/m²
225 ft-lb/in²
Type S; ASTM D1822
SABIC Innovative Plastics Lexan® LS1 PC (Asia Pacific)
Automotive lens applications. Low viscosity. UV-stabilized. Transparent colors only.
Tensile Impact Strength 472 kJ/m²
225 ft-lb/in²
Type S; ASTM D 1822
SABIC Innovative Plastics Lexan® OQ2220 PC
Ophthalmic/safety lens market. OQ2xxx series in all transparent tints. Dedicated equipment, stringent production control conditions.This data was supplied by SABIC-IP for the Americas region.