Polymer Property : Tensile Impact Strength = 231 kJ/m² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Impact Strength 231 kJ/m²
110 ft-lb/in²
23°C; ASTM D-1822
ExxonMobil Escorene® LL-5002 LLDPE Compounding Resin  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A linear low density polyethylene resin designed to provide good processability and ease of blending. LL-5002 also exhibits good toughness and envi..
Tensile Impact Strength 231 kJ/m²
110 ft-lb/in²
ASTM D1822
ExxonMobil HDPE AA48-002 High Density Polyethylene Resin
Product Description: AA48-002 is a blow molding grade high density polyethylene copolymer containing an antistatic additive. It provides a very good balance of stress crack resistance, stiffness and..
Tensile Impact Strength 231 kJ/m²
110 ft-lb/in²
ASTM D1822
ExxonMobil Paxon™ AA45-004 Blow Molding Resin
Product Description: AA45-004 is a blow molding high density polyethylene copolymer offering exceptional stress cracking resistance and impact performance.Availability: Latin America, North America ..
Tensile Impact Strength 231 kJ/m²
110 ft-lb/in²
ASTM D1822
ExxonMobil Paxon™ AG45-004 Blow Molding Resin  (discontinued **)
AG45-004 is a blow molding high density polyethylene which offers exceptional stress crack resistance and impact performance. It contains an antistat which permits this resin to be used in all food..