Polymer Property : Tensile Impact Strength = 234 ft-lb/in² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Impact Strength 491 kJ/m²
234 ft-lb/in²
At 23°C; ASTM D1822S
DuPont Nucrel® 699 Ethylene-Methacrylic Acid Copolymer Resin
Nucrel® 599 is a tough, lightweight, easily processed ethylene copolymer resin. This resin is inherently flexible without the need for plasticizers. The resin can be pigmented, UV-stabilized for ..