Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Impact Strength = 240 kJ/m² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Impact Strength 240 kJ/m²
114 ft-lb/in²
Type S bar; ASTM D1822
Chevron Phillips Marlex® K605 HDPE Blow Molding Resin
Resin Type: Ethylene HomopolymerCharacteristics: Good ESCRExceptional rigidityExcellent melt strengthApplications: Automotive bumper beamsInformation provided by Chevron Phillips.
Copyright © lookpolymers.com All Rights Reserved