Tensile Impact Strength 567 kJ/m²
270 ft-lb/in²
ASTM D1822
Styron CALIBREâ„¢ 2061-6 Polycarbonate Resin
Overview: CALIBREâ„¢ 2061-6 resin is suitable for steam and ethylene oxide sterilization required by the health care industry. CALIBRE 2061-6 provides excellent heat resistance, impact strength, ..
Tensile Impact Strength 567 kJ/m²
270 ft-lb/in²
ASTM D1822
Styron CALIBREâ„¢ MEGARAD 2081-6LR Polycarbonate Resin
Overview: CALIBREâ„¢ 2081-6LR Polycarbonate resin was developed for medical applications requiring improved resistance to lipids over standard polycarbonate resins. When exposed to a 20% intralip..
Tensile Impact Strength 567 kJ/m²
270 ft-lb/in²
ASTM D1822
ExxonMobil Paxon™ BA53-035 Blow Molding Resin  (discontinued **)