Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Impact Strength | 570 kJ/m² | 271 ft-lb/in² | 23°C; ASTM D-1822 |
ExxonMobil Iotek® 8000 Sodium Ionomer Molding/Extrusion Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A sodium ionomer with excellent abrasion resistance, impact strength, hardness and tensile strength. IOTEK ionomers provide superb low temperature .. |