Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Impact Strength | 577 kJ/m² | 275 ft-lb/in² | Type S; ASTM D1822 |
SABIC Innovative Plastics Lexan® 144 PC UL rated HB. 200 series recommended when V-2 rating required. 10.5 MFR. FDA food contact compliant in limited colors.Effective January 15th, 2007 this grade will no longer be supported with bioco.. |
|||
Tensile Impact Strength | 577 kJ/m² | 275 ft-lb/in² | Type S; ASTM D1822 |
SABIC Innovative Plastics Lexan® 241 PC (Asia Pacific) 10.5 MFR. Improved flame retardance. |
|||
Tensile Impact Strength | 577 kJ/m² | 275 ft-lb/in² | Type S; ASTM D1822 |
SABIC Innovative Plastics Lexan® 241R PC General purpose polycarbonate with 10.5 MFR and internal mold release. |
|||
Tensile Impact Strength | 577 kJ/m² | 275 ft-lb/in² | Type S; ASTM D1822 |
SABIC Innovative Plastics Lexan® 241R PC (Asia Pacific) 10.5 MFR. Improved flame retardance. Internal mold release. |
|||
Tensile Impact Strength | 578 kJ/m² | 275 ft-lb/in² | Type S; ASTM D1822 |
SABIC Innovative Plastics Lexan® 244R PC 10.5 MFR. Improved flame retardance. USA FDA compliant (limited colors). Internal mold release. |
|||
Tensile Impact Strength | 577 kJ/m² | 275 ft-lb/in² | Type S; ASTM D1822 |
SABIC Innovative Plastics Lexan® 4501 PPC (Asia Pacific) High heat resistant polyphthlate carbonate, provides DTUL of 290F at 264 psi. |
|||
Tensile Impact Strength | 577 kJ/m² | 275 ft-lb/in² | Type S; ASTM D1822 |
SABIC Innovative Plastics Lexan® 4504 PPC High heat resistant polycarbonate copolymer, provides DTUL of 290F at 264 psi. FDA food contact compliant in limited colors. Effective January 15th, 2008 this grade will no longer be supported with .. |
|||
Tensile Impact Strength | 577 kJ/m² | 275 ft-lb/in² | Type S; ASTM D1822 |
SABIC Innovative Plastics Lexan® 4504 PPC (Asia Pacific) High heat resistant polycarbonate copolymer, provides DTUL of 290F at 264 psi. FDA food contact compliant in limited colors. Effective January 15th, 2008 this grade will no longer be supported wit.. |
|||
Tensile Impact Strength | 577 kJ/m² | 275 ft-lb/in² | Type S; ASTM D1822 |
SABIC Innovative Plastics Lexan® 4701R PPC High heat resistant polyphthlate carbonate, provides DTUL of 300F at 264 psi. |
|||
Tensile Impact Strength | 577 kJ/m² | 275 ft-lb/in² | Type S; ASTM D1822 |
SABIC Innovative Plastics Lexan® 4701R PPC (Asia Pacific) High heat resistant polyphthlate carbonate, provides DTUL of 300F at 264 psi. |
|||
Tensile Impact Strength | 577 kJ/m² | 275 ft-lb/in² | Type S; ASTM D1822 |
SABIC Innovative Plastics Lexan® 4704 PPC (Asia Pacific) High heat resistant polycarbonate copolymer, provides DTUL of 300F at 264 psi. FDA food contact compliant in limited colors. Effective January 15th, 2008 this grade will no longer be supported with .. |
|||
Tensile Impact Strength | 577 kJ/m² | 275 ft-lb/in² | Type S; ASTM D1822 |
SABIC Innovative Plastics Lexan® HP4R PC Medium flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). ETO and steam sterilizable. Contains a h.. |
|||
Tensile Impact Strength | 577 kJ/m² | 275 ft-lb/in² | Type S; ASTM D1822 |
SABIC Innovative Plastics Lexan® HPH4404 PPC+PC (Europe-Africa-Middle East) High heat specialty polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam, gamma and e-beam steril.. |
|||
Tensile Impact Strength | 577 kJ/m² | 275 ft-lb/in² | Type S; ASTM D 1822 |
SABIC Innovative Plastics Lexan® HPH4504 PPC High heat specialty polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 of USP Class VI). EtO, steam, gamma and e-beam steril.. |
|||
Tensile Impact Strength | 577 kJ/m² | 275 ft-lb/in² | Type S; ASTM D1822 |
SABIC Innovative Plastics Lexan® HPH4504 PPC (Asia Pacific) High heat specialty polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 of USP Class VI). EtO, steam, gamma and e-beam steril.. |
|||
Tensile Impact Strength | 577 kJ/m² | 275 ft-lb/in² | Type S; ASTM D1822 |
SABIC Innovative Plastics Lexan® HPH4504H PPC (Asia Pacific) High heat specialty polycarbonate with enhanced autoclavability. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 of USP Class VI). EtO, .. |
|||
Tensile Impact Strength | 577 kJ/m² | 275 ft-lb/in² | Type S; ASTM D 1822 |
SABIC Innovative Plastics Lexan® HPH4504H PPC (Europe-Africa-Middle East) High heat specialty polycarbonate with enhanced autoclavability. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 of USP Class VI). EtO, .. |
|||
Tensile Impact Strength | 577 kJ/m² | 275 ft-lb/in² | Type S; ASTM D1822 |
SABIC Innovative Plastics Lexan® HPH4504HEU PPC (Europe-Africa-Middle East) High heat specialty polycarbonate with enhanced autoclavability. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 of USP Class VI). EtO, .. |
|||
Tensile Impact Strength | 577 kJ/m² | 275 ft-lb/in² | Type S; ASTM D1822 |
SABIC Innovative Plastics Lexan® HPH4704 PPC (Asia Pacific) High heat specialty polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam, gamma and e-beam steril.. |
|||
Tensile Impact Strength | 577 kJ/m² | 275 ft-lb/in² | Type S; ASTM D 1822 |
SABIC Innovative Plastics Lexan® IR2240 PC UL rated HB. 200 series recommended when V-2 rating required. Nonhalogenated. MFR 10.5. Internal mold release. FDA food contact compliant in limited colors.This data was supplied by SABIC-IP for.. |
|||
Tensile Impact Strength | 577 kJ/m² | 275 ft-lb/in² | Type S; ASTM D1822 |
SABIC Innovative Plastics Lexan® LS2 PC UL rated HB as of 10/97. 200 series recommended when V-2 rating required. Automotive lens applications. Medium viscosity. UV-stabilized. Transparent colors only. |
|||
Tensile Impact Strength | 577 kJ/m² | 275 ft-lb/in² | Type S; ASTM D1822 |
SABIC Innovative Plastics Lexan® LS2 PC (Asia Pacific) Automotive lens applications. Medium viscosity. UV-stabilized. Transparent colors only. |
|||
Tensile Impact Strength | 577 kJ/m² | 275 ft-lb/in² | Type S; ASTM D 1822 |
SABIC Innovative Plastics Lexan® PPC4701 PPC High heat resistant polyphthlate carbonate, provides DTUL of 300F at 264 psi.This data was supplied by SABIC-IP for the Americas region. |
|||
Tensile Impact Strength | 577 kJ/m² | 275 ft-lb/in² | Type S; ASTM D1822 |
SABIC Innovative Plastics Lexan® 141R PC (Asia Pacific) Nonhalogenated. 10.5 MFR. Internal mold release. |
|||
Tensile Impact Strength | 577 kJ/m² | 275 ft-lb/in² | Type S; ASTM D 1822 |
SABIC Innovative Plastics Lexan® 141S PC (Asia Pacific) Nonhalogenated. 10.5 MFR. Internal mold release.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Tensile Impact Strength | 577 kJ/m² | 275 ft-lb/in² | Type S; ASTM D1822 |
SABIC Innovative Plastics Lexan® 144 PC (Asia Pacific) LEXAN 144 is a medium viscosity multi purpose grade. FDA food contact compliant in limited colors. Effective January 15th, 2007 this grade is no longer supported with biocompatibility information .. |
|||
Tensile Impact Strength | 577 kJ/m² | 275 ft-lb/in² | Type S; ASTM D1822 |
SABIC Innovative Plastics Lexan® 144R PC (Asia Pacific) LEXAN 144R is a medium viscosity multi purpose grade. FDA food contact compliant in limited colors. Effective January 15th, 2007 this grade is no longer supported with biocompatibility information.. |
|||
Tensile Impact Strength | 577 kJ/m² | 275 ft-lb/in² | Type S; ASTM D1822 |
SABIC Innovative Plastics Lexan® 4501 PPC High heat resistant polyphthlate carbonate, provides DTUL of 290F at 264 psi. |
|||
Tensile Impact Strength | 577 kJ/m² | 275 ft-lb/in² | Type S; ASTM D1822 |
SABIC Innovative Plastics Lexan® HPH4704 PPC (Europe-Africa-Middle East) High heat specialty polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam, gamma and e-beam steril.. |
|||
Tensile Impact Strength | 577 kJ/m² | 275 ft-lb/in² | Type S; ASTM D1822 |
SABIC Innovative Plastics Lexan® HP4NR PC Medium flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains no m.. |