Mechanical Properties Metric English Comments
Tensile Impact Strength 280 kJ/m²
133 ft-lb/in²
Notched, 23°C; ISO 8256
Total Finathene® 53080 HDPE, blow molding, sheet  (discontinued **)
Finathene E® 53080 is a high density polyethylene produced by the slurry loop low pressure polymerization process. Finathene E® 53080 has been especially developed for the production of containers..