Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Impact Strength | 640 kJ/m² | 305 ft-lb/in² | Type S; ASTM D1822 |
SABIC Innovative Plastics Lexan® OQ2720 PC Ophthalmic/safety lens market. OQ2xxx series in all transparent tints. Dedicated equipment, stringent production control conditions. |
|||
Tensile Impact Strength | 640 kJ/m² | 305 ft-lb/in² | Type S; ASTM D1822 |
SABIC Innovative Plastics Lexan® OQ2720 PC (Asia Pacific) Ophthalmic/safety lens market. OQ2xxx series in all transparent tints. Dedicated equipment, stringent production control conditions. |