Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Impact Strength | 330 kJ/m² | 157 ft-lb/in² | |
LyondellBasell Lupolen® 5261 Z HI HDPE Data was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell. |