Polymer Property : Tensile Impact Strength = 34.0 kJ/m² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Impact Strength 34.0 kJ/m²
16.2 ft-lb/in²
ASTM D1822
Chevron Phillips HiD® 9055 HDPE Injection Molding Resin  (discontinued **)
Resin Type: Linear Copolymer, ASTM D 4976 Classification: PE 231, A 52600Characteristics: Excellent Flow, Moderate Impact Strength, Good Stiffness, Moderate ESCR, Excellent Shrinkage ResistanceAppli..
Tensile Impact Strength 34.0 - 330 kJ/m²
16.2 - 157 ft-lb/in²
Average value: 123 kJ/m² Grade Count:9
Overview of materials for High Density Polyethylene (HDPE), Injection Molded
This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Injection Molded". Each property range of values reported is minimum a..