Polymer Property : Tensile Impact Strength = 34.0 ft-lb/in²
Polymer Property :
Tensile Impact Strength =
34.0 ft-lb/in²
Product List
Mechanical Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties
Metric
English
Comments
Tensile Impact Strength
71.4
kJ/m²
34.0
ft-lb/in²
ASTM D1822
Network Polymers NPP 50-0350
Description: High Density Polyethylene (HDPE)Information provided by Network Polymers Inc.