Mechanical Properties Metric English Comments
Tensile Impact Strength 75.0 kJ/m²
35.7 ft-lb/in²
LyondellBasell Lupolen® 5031 L HDPE, Injection Molding Grade
Easy flow, injection molding grade for closures, aerosol pumps, spray nozzles for spray cans, small automotive parts such as the caps on lead/acid batteries, knobs, barrels for writing instruments a..