Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Impact Strength | 860 kJ/m² | 409 ft-lb/in² | ASTM D1822S |
DuPont™ Surlyn® 8920 Ionomer Resin, Sodium Surlyn® 8920 thermoplastic resin is an advanced ethylene/methacrylic acid (E/MAA) copolymer, in which the MAA acid groups have been partially neutralized with sodium ions. The amount of MAA and neu.. |
|||
Tensile Impact Strength | 860 kJ/m² | 409 ft-lb/in² | ASTM D1822S |
DuPont™ Surlyn® PC100 Ionomer Resin, Highest Clarity, Sodium Surlyn® PC100 luxury molding resin is a "select" grade of Surlyn® 8920, controlled to achieve the highest possible optical clarity in molded perfume jars and caps. It complies with the provisions .. |