Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Impact Strength | 426 kJ/m² | 203 ft-lb/in² | |
Kraton® D1102 + LDPE blend (50/50) Blending KRATON D and G polymers with PE significantly improves the toughness at both room and low temperatures. KRATON polymers are block segments of styrene and rubber monomers (A-B, A-B-A, or [A.. |