Polymer Property : Tensile Impact Strength = 52.3 ft-lb/in² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Impact Strength 110 - 280 kJ/m²
52.3 - 133 ft-lb/in²
Average value: 167 kJ/m² Grade Count:5
Overview of materials for Acetal Copolymer, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Unreinforced". Each property range of values reported is minimum and maximum values of..
Tensile Impact Strength 110 kJ/m²
52.3 ft-lb/in²
ASTM D1822
Global POM-270 Low Melt Acetal
Information provided by Global Polymers Corporation.
Tensile Impact Strength 110 kJ/m²
52.3 ft-lb/in²
Notched, -30°C; ISO 8256
Total Finathene® SI 508 HDPE blow molding  (discontinued **)
Finathene® SI 508 is part of a new generation of high density ethylene-hexene copolymers produced by the slurry loop low pressure polymerization process. Finathene® SI 508 is a high molecular weig..