Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Impact Strength 672 kJ/m²
320 ft-lb/in²
ASTM D1822, Type S
Dow AMPLIFY™ EA 101 Ethylene-ethyl Acrylate (EEA)
AMPLIFY™ EA 101 Functional Polymer is produced via a high pressure reactor. It exhibits high flexibility and imparts low temperature toughness to a wide range of engineering resins. This polymer..