Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Impact Strength | 732 kJ/m² | 348 ft-lb/in² | 23°C; ASTM D-1822 |
ExxonMobil Escorene® LD-701 High EVA Film Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A fractional melt, 10.5% vinyl acetate copolymer specialty film resin for applications requiring outstanding heat sealability, strength and toughnes.. |
|||
Tensile Impact Strength | 732 kJ/m² | 348 ft-lb/in² | 23°C; ASTM D-1822 |
ExxonMobil Escorene® LD-705 High EVA Film Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A fractional melt index, 13.3% vinyl acetate copolymer specialty film resin for applications requiring outstanding heat sealability, strength, and t.. |