Polymer Property : Tensile Impact Strength = 9.50 kJ/m² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Impact Strength 9.50 kJ/m²

@Temperature -40.0 °C
4.52 ft-lb/in²

@Temperature -40.0 °F
ASTM D1822S
DuPont Nucrel® 2940 Ethylene-Methacrylic Acid Copolymer Resin  (discontinued **)
Nucrel® 2940is a tough, lightweight, easily processed ethylene copolymer resin. This resin is inherently flexible without the need for plasticizers. The resin can be pigmented, UV-stabilized for ..