Mechanical Properties Metric English Comments
Tensile Impact Strength 190 kJ/m²
90.4 ft-lb/in²
Type S bar; ASTM D1822
Polymer Industries Densetec HMW Sheet
Polymer Industries’ Densetec HMW is the extruded material needed when Densetec HDPE is not enough and Polyslick UHMW™ is not necessary. Densetec HMW has higher impact strength than HDPE and is mor..