Mechanical Properties Metric English Comments
Tensile Impact Strength 95.0 kJ/m²
45.2 ft-lb/in²
S bar; ASTM D 1822
Chevron Phillips Marlex® 9512H - 9513H High Performance Series HDPE Blow Molding Resin
Resin Type: linear copolymerCharacteristics: excellent physical properties, medium molecular weight distribution, wide range of processing conditions, good flow for injection blow molding applicatio..