Polymer Property : Tensile Creep Modulus, 1 hour = 10100 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Creep Modulus, 1 hour 10100 MPa
1.46e+6 psi
Covestro Makrolon® 8325 Polycarbonate
High viscosity injection molding and extrusion grade with 20% standard glass fibers and easy mold release, high strength and stiffness.Information provided by Bayer.As of 1 September 2015, Bayer Mat..