Polymer Property : Tensile Creep Modulus, 1 hour = 239000 psi
Polymer Property :
Tensile Creep Modulus, 1 hour =
239000 psi
Product List
Mechanical Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties
Metric
English
Comments
Tensile Creep Modulus, 1 hour
1650
MPa
239000
psi
ISO 899-1
Lanxess Pocan® S 1517 000000 PBT
PBT, non-reinforced, injection molding, extrusion, impact modified