Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Creep Modulus, 1 hour | 260 MPa | 37700 psi | |
LyondellBasell Lupolen® UHM 201 MDPE, Ultra-High Molecular Weight For the production of very high abrasion and impact resistant parts with lower slip/stick friction, as well as higher stress crack and chemical resistance. Apart from anticorrosion products, this m.. |
|||
Tensile Creep Modulus, 1 hour | 260 MPa | 37700 psi | |
LyondellBasell Lupolen® UHM 301 MDPE, Ultra-High Molecular Weight For the production of very high abrasion and impact resistant parts with lower slip/stick friction, as well as higher stress crack and chemical resistance. Apart from anticorrosion products, this m.. |
|||
Tensile Creep Modulus, 1 hour | 260 MPa @Time 3600 sec |
37700 psi @Time 1.00 hour |
ISO 899-1 |
DuPont Performance Polymers Hytrel® 6646 NC010 Polyester Elastomer TPC-ET
(Unverified Data**) 66 Shore D High Performance Polyester ElastomerInformation provided by DuPont Performance Polymers |