Polymer Property : Tensile Creep Modulus, 1 hour = 310000 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Creep Modulus, 1 hour 2140 MPa
310000 psi
Arkema Group Orgalloy® R 6600 Nylon 66 Alloy, Rigid Grade (Conditioned)
Rigid polyamide 6.6 alloy: easy to process, low moisture absorption, chemical resistance (no known solvents).ISO data provided by the manufacturer, Arkema.