Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Creep Modulus, 1 hour 3600 - 11000 MPa
522000 - 1.60e+6 psi
Average value: 9640 MPa Grade Count:9
Overview of materials for Polybutylene Terephthalate (PBT), 30% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 30% Glass Fiber Filled". Specific grades with glass content between 25..
Tensile Creep Modulus, 1 hour 3600 MPa
522000 psi
ISO 899-1
Covestro Makrolon® 9415 Polycarbonate, 10% Glass Filled
ISO 7391-PC,MFR,(,,)-09-9,GF10Global gradeMVR (300 °C/1.2 kg) 6.0 cm3/10 min10 % Glass fiber reinforcedChlorine- and bromine-free flame retardantUL 94V-0/1.5 mm and 5VA/3.0 mmHigh viscosityEasy rel..
Tensile Creep Modulus, 1 hour 3600 MPa
522000 psi
ISO 899-1
Covestro Makrolon® 9417 Polycarbonate, 10% Glass Filled
ISO 7391-PC,MFLR,(,,)-09-9,GF10Global gradeMVR (300 °C/1.2 kg) 6.0 cm3/10 min10 % Glass fiber reinforcedChlorine- and bromine-free flame retardantUL 94V-0/1.5 mm and 5VA/3.0 mmHigh viscosityUV stab..