Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Creep Modulus, 1 hour 550 - 700 MPa
79800 - 102000 psi
Average value: 657 MPa Grade Count:7
Overview of materials for Polypropylene, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Molded". Each property range of values reported is minimum and maximum values of appropri..
Tensile Creep Modulus, 1 hour 550 MPa
79800 psi
BASF Novolen® 2300 L Polypropylene
Injection molded parts.Data was collected by ISO methods and provided by BASF.
Tensile Creep Modulus, 1 hour 550 MPa
79800 psi
BASF Novolen® 2500 H Polypropylene
Injection molded parts, blow moldings and thermoformed parts.Data was collected by ISO methods and provided by BASF.