Tensile Creep Modulus, 1 hour 3500 - 7300 MPa
508000 - 1.06e+6 psi
Average value: 6020 MPa Grade Count:12
Overview of materials for Polybutylene Terephthalate (PBT), 20% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 20% Glass Fiber Filled". Specific grades with glass content between 15..