Polymer Property : Modulus of Elasticity = 0.00225 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Modulus of Elasticity 0.00225 GPa
0.326 ksi
After 7 days at 70°C; ASTM D412 ISO 37
Advanced Polymer Alloys DuraGrip™ 6160 BK Melt Processable Elastomer
DuraGrip™ 6160BK is designed to be a special purpose Melt Processable Elastomer (MPE) that is easy to use in injection molding and extrusion processes. DGR 6160BK has an excellent soft touch feel a..