Polymer Property : Modulus of Elasticity = 0.00603 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Modulus of Elasticity 0.00603 GPa
0.875 ksi
Silicone Property; Arlon SQA-TMS-008
Arlon Thermabond® 48991A010 0.010" (0.254 mm) Uncured Silicone Rubber with Fiberglass Substrate
Description: Generation IIa Thermabond® NP electrically insulating electronic adhesive. Bonds without primer.Design/Construction: Liner: PolyethyleneSide 1: Uncured Silicone RubberSubstrate: Style ..
Modulus of Elasticity 0.00603 GPa
0.875 ksi
Silicone Property; Arlon SQA-TMS-008
Arlon Thermabond® 48991A015 0.015" (0.381 mm) Uncured Silicone Rubber with Fiberglass Substrate
Description: Thermabond® G2pr - electrically insulating electronic adhesive. Bonds without primer.Design/Construction: Liner: PolyethyleneSide 1: Uncured Silicone RubberSubstrate: Style 1080 Fiberg..
Modulus of Elasticity 0.00603 GPa
0.875 ksi
Silicone Property; ASTM E 831
Arlon R36601A010 0.010" (0.254 mm) Uncured Silicone Rubber with Fiberglass Substrate
Description: Generation II Thermabond® NP electrically insulating electronic adhesive. Bonds without primer.Design/Construction: Liner 1: Polyethylene Side 1: Uncured Silicone Rubber Substrate: Sty..