Polymer Property : Modulus of Elasticity = 0.0130 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Modulus of Elasticity 0.0130 - 10.5 GPa
1.89 - 1520 ksi
Average value: 0.426 GPa Grade Count:68
Overview of materials for Polyester Thermoplastic Elastomer
This property data is a summary of similar materials in the MatWeb database for the category "Polyester Thermoplastic Elastomer". Each property range of values reported is minimum and maximum values..
Modulus of Elasticity 0.0130 - 30.1 GPa
1.89 - 4370 ksi
Average value: 13.7 GPa Grade Count:136
Overview of materials for Nylon 6, 50% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 50% Glass Fiber Filled". Specific grades with glass content between 45% and 54% are included. E..
Modulus of Elasticity 0.0130 GPa
1.89 ksi
DuPont Elvax® 260 Ethylene-Vinyl Acetate Copolymer Resin
Elvax resins offer a unique combination of processing and performance characteristics. They provide outstanding toughness and resilience and maintain flexibility over a broad temperature range with..