Mechanical Properties Metric English Comments
Modulus of Elasticity 0.0197 GPa
2.85 ksi
3M Jet-Weld™ TE-040 Adhesive
A warm applied, moisture-curing polyurethane adhesive for wood working, laminating and plastic component assembly.Extrudable. Fast set time, low viscosity, and strong, flexible bonds for a wide vari..