Polymer Property : Modulus of Elasticity = 0.01991 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Modulus of Elasticity 0.01991 GPa
2.887 ksi
Calculated; ASTM D412 Method A
Seals Eastern 7352D Nano-PTFE Filled Fluoroelastomer
Nano-PTFE filled fluoroelastomer for low wear in hot dynamic applicationsInformation provided by Seals Eastern.