Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 0.0441 GPa | 6.40 ksi | Silicone Property; Arlon-SAQ-TMS-008 |
Arlon Thermabond® T-20 NP (99770W015) 0.015" (0.381 mm) Uncured Silicone Rubber with PTFE Coated Fiberglass Carrier Description: 15 mil Primerless Thermabond®. T-20 NP. Thermally conductive, electrically insulating electronic adhesive. Bonds with primer.Design/Construction:Liner: FEPProduct: Uncured Silicone Rub.. |