Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 0.0483 GPa | 7.00 ksi | Arlon SQA-TMS-008 |
Arlon Thermabond® 99720W015 0.015" Uncured Silicone Rubber with PTFE Coated Fiberglass Carrier Design/Construction:Liner: 0.001" FEP FilmSide 1: Uncured Silicone RubberCarrier: 0.003" PTFE coated FiberglassRecommended Primer: Dow Corning S2260This data represents typical values for the pr.. |