Polymer Property : Modulus of Elasticity = 0.0621 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Modulus of Elasticity 0.0621 GPa
9.00 ksi
Arlon SQA-TMS-008
Arlon Thermabond® R37340X008 Primerless Electronic Adhesive  (discontinued **)
Liner: 1 mil FEP; Product: uncured Silicone Rubber; Carrier: 3 mil PTFE coated fiberglas
Modulus of Elasticity 0.0621 GPa
9.00 ksi
1% strain, Silicone Property; Arlon SQA-TMS-008
Arlon Thermabond® 99A90N008 Primerless Electronic Adhesive  (discontinued **)
Electrically insulating, thermally conductive, electronic adhesive. Bonds without primer.