Mechanical Properties Metric English Comments
Modulus of Elasticity 0.0180 - 0.0800 GPa
2.61 - 11.6 ksi
Average value: 0.0474 GPa Grade Count:9
Overview of materials for Ethylene-Methyl Acrylate Copolymer, Molding Grade
This property data is a summary of similar materials in the MatWeb database for the category "Ethylene-Methyl Acrylate Copolymer, Molding Grade". Each property range of values reported is minimum an..