Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 0.228 GPa | 33.1 ksi | Secant; ASTM D638 |
Huntsman PE1407 EVA Film Extrusion
(discontinued **) 4% Vinyl Acetate EVA copolymer and FDA compliantFeatures: Excellent balance of optical and strength, toughness and flexibility at low temperatures, and good heat seal characteristic.Applications: Fi.. |
|||
Modulus of Elasticity | 0.228 GPa | 33.1 ksi | Secant; ASTM D638 |
Huntsman PE2030 Injection Molding Polyethylene
(discontinued **) Homopolymer, Drug Master File listed product, and FDA compliant.Features: High mechanical flexing properties, excellent processability, good stress crack resistance, and very good low temperature st.. |